Effect of enamel surface pretreatment and thermocycling on shear bond strength of metallic orthodontic brackets bonded with a self-adhesive resin: An in vitro study - 19/11/26

Doi : 10.1016/j.ortho.2026.101274 
Ingrid Silva De Lima 1 , Isadora Da Silva Ximenes 1 , Vitor Hugo Queiroz de Barros 1 , Ranyele Elis Alexandre Rodrigues 1 , Ketelyn Kerty Moreira de Oliveira 1 , Vitaliano Gomes de Araújo-Neto 2 , Anderson Gomes Forte 2 , Tainah Oliveira Rifane 1, ⁎ , Alexandre Daher Yunes Salgado 1
1 Paulo Picanço School of Dentistry, Fortaleza, Ceará, Brazil 
2 Department of Dental Materials, Piracicaba Dental School (FOP), University of Campinas (UNICAMP), Piracicaba, SP, Brazil 

⁎ Tainah Oliveira Rifane, Paulo Picanço School of Dentistry, 900 Joaquim Sá St., Fortaleza, Ceará, Brazil. Paulo Picanço School of Dentistry 900 Joaquim Sá St. Fortaleza Ceará Brazil

Highlights

•
Airborne-particle abrasion (50-mm aluminium oxide particles at 2 bars, at 1 cm, for 10 s) significantly increased orthodontic bracket bond strength.
•
Self-adhesive resin showed improved adhesion after enamel air abrasion.
•
Thermocycling significantly reduced bond strength in all experimental groups.
•
Combined acid etching and air abrasion did not outperform air abrasion alone.
•
Air abrasion promoted more favourable adhesive failure patterns after debonding.

Le texte complet de cet article est disponible en PDF.

Summary

Objective

This study evaluated the effect of different enamel surface treatments on the microshear bond strength and failure mode of orthodontic brackets bonded with a self-adhesive orthodontic resin before and after thermocycling.

Materials and methods

Bovine enamel specimens were embedded in polyvinyl chloride tubes with chemically activated acrylic resin and allocated into four groups according to enamel surface treatment: self-adhesive resin (SAR), acid etching + SAR, airborne-particle abrasion + SAR, and acid etching + airborne-particle abrasion + SAR. Each group was divided into immediate and aged conditions ( n = 10). Acid etching was performed with 37% phosphoric acid for 30 s, and airborne-particle abrasion with 50-μm aluminium oxide for 10 s. Brackets were bonded using Ortholink One Step adhesive. Aged specimens underwent 20,000 thermal cycles (5–55 °C). Microshear bond strength was measured using a universal testing machine, and failure mode was assessed with the Adhesive Remnant Index. Data were analysed using Tukey's test (α = 0.05).

Results

Both surface treatment and thermocycling significantly influenced bond strength. In the immediate condition, air-abraded groups showed the highest bond strength (8.16–8.55 MPa), significantly exceeding non-abraded groups (5.17–5.30 MPa; P < 0.001). After thermocycling, air-abraded groups maintained higher bond strength (5.24–5.89 MPa) than the self-adhesive resin group (2.57 ± 1.04 MPa; (F(1,41) = 42.68, P < 0.001). Thermocycling significantly reduced bond strength in all groups ( P ≤ 0.049). Non-air-abraded groups exhibited only ARI score 0 failures, whereas air-abraded groups showed mixed failure patterns.

Conclusion

Airborne-particle abrasion significantly improved bracket bond strength to intact enamel when using a self-adhesive orthodontic resin, although thermocycling reduced adhesion regardless of surface treatment.

Le texte complet de cet article est disponible en PDF.

Keywords : Orthodontic brackets, Enamel, Self-adhesive resin, Air abrasion, Aluminum oxide, Bond strength


Plan


© 2026  The Authors. Publié par Elsevier Masson SAS. Tous droits réservés.
Ajouter à ma bibliothèque Retirer de ma bibliothèque Imprimer
Export

    Export citations

  • Fichier

  • Contenu

Vol 25 - N° 1

Article 101274- mars 2027 Retour au numéro

Bienvenue sur EM-consulte, la référence des professionnels de santé.
L’accès au texte intégral de cet article nécessite un abonnement.

Déjà abonné à cette revue ?

Elsevier s'engage à rendre ses eBooks accessibles et à se conformer aux lois applicables. Compte tenu de notre vaste bibliothèque de titres, il existe des cas où rendre un livre électronique entièrement accessible présente des défis uniques et l'inclusion de fonctionnalités complètes pourrait transformer sa nature au point de ne plus servir son objectif principal ou d'entraîner un fardeau disproportionné pour l'éditeur. Par conséquent, l'accessibilité de cet eBook peut être limitée. Voir plus

Mon compte


Plateformes Elsevier Masson

Déclaration CNIL

EM-CONSULTE.COM est déclaré à la CNIL, déclaration n° 1286925.

En application de la loi nº78-17 du 6 janvier 1978 relative à l'informatique, aux fichiers et aux libertés, vous disposez des droits d'opposition (art.26 de la loi), d'accès (art.34 à 38 de la loi), et de rectification (art.36 de la loi) des données vous concernant. Ainsi, vous pouvez exiger que soient rectifiées, complétées, clarifiées, mises à jour ou effacées les informations vous concernant qui sont inexactes, incomplètes, équivoques, périmées ou dont la collecte ou l'utilisation ou la conservation est interdite.
Les informations personnelles concernant les visiteurs de notre site, y compris leur identité, sont confidentielles.
Le responsable du site s'engage sur l'honneur à respecter les conditions légales de confidentialité applicables en France et à ne pas divulguer ces informations à des tiers.


Tout le contenu de ce site: Copyright © 2026 Elsevier, ses concédants de licence et ses contributeurs. Tout les droits sont réservés, y compris ceux relatifs à l'exploration de textes et de données, a la formation en IA et aux technologies similaires. Pour tout contenu en libre accès, les conditions de licence Creative Commons s'appliquent.